Abstract

It has been shown previously that high levels of residual monomer have a deleterious effect on the properties of denture base polymers. Levels of residual monomer were determined on a homopolymer and a copolymer using gas-liquid chromatography. A wide range of recommended and ‘short cut’ curing cycles were then investigated which produced values ranging from 0.56 to 18.46%. From the ranges examined an optimum cycle of 7 h at 70°C and 1 h at 100°C was established which was used to polymerize 23 currently available synthetic denture base polymers. Only small differences were found between the materials tested with a range from 0.54 to 1.08% of residual monomer.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.