Abstract

PbTe/Ag composite powders were synthesized by a chemical plating method and then compacted by spark plasma sintering (SPS) at 573 K to 673 K and 50 MPa. The effects of the sintering temperature on the thermoelectric properties of PbTe and the PbTe/Ag composites were investigated. The thermoelectric properties of PbTe and PbTe/Ag bulk samples were measured in the temperature range from 300 K to 700 K. PbTe/Ag bulk samples changed electrical transport behavior from p-type to n-type at room temperature. The SPS temperature not only changed the lattice parameter but also affected the conduction behavior of PbTe/Ag composites. The variation in the carrier concentration was determined by the role of the Ag dopant for different SPS temperatures. Moreover, the conduction of the PbTe/Ag samples changed from metallic to semiconducting in the measured temperature range from 300 K to 700 K as the sintering temperature increased. For the PbTe/Ag bulk materials subjected to SPS at 573 K and 673 K, the values of the power factor were 0.38 mW/m K2 and 1.31 mW/m K2 at 700 K, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.