In this work, we studied the effect of sintering temperature (1100 - 1400 °C) and thermomagnetic treatment (TMT) on the magnetic hysteresis characteristics of the Fe-30Cr-8 Co alloy, obtained by powder technology. It has been shown that at sintering temperatures of 1200 °C and below, it is possible to obtain materials with high magnetic characteristics that ensure their technical application. Properties exceed the characteristics of analogues obtained by casting technology. In the range 1200 - 1250 °C, the largest increase in the density of samples is observed with an increase in sintering temperature with a simultaneous increase in the values of magnetic characteristics. It was revealed that the total duration of heat treatment for 40-80 hours is sufficient for the formation of the necessary structure that determines the magnetic properties of the material. Long-term heat treatment (up to 160 hours) contributes to a higher level of magnetic properties.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call