In this study, we investigated various sintering temperatures (1200 °C−1450 °C) and durations (2–6 h) conditions for preparing (Tb1/2Nb1/2)0.01Ti0.99O2 (TNTO) ceramics. By employing high sintering temperatures (≥1350 °C) and extended sintering durations (≥4 h), we successfully achieved ultra–high dielectric permittivity values (ε′ ∼ 2.2 − 4.1 × 104) and remarkably low loss tangent values (∼0.025−0.079). Remarkably, the temperature coefficient of the TNTO ceramic, sintered at 1350 °C, exhibited exceptional stability, maintaining a value of approximately 15% even at 200 °C. Additionally, we examined the phase structure and microstructure of the TNTO ceramics to gain insights into their colossal permittivity (CP) behavior. The analysis revealed the presence of rutile TiO2 and TbNbTiO6 phases, and the ceramics exhibited a high–density microstructure under high–temperature sintering conditions. The impedance spectroscopy analysis revealed that the primary contributor to the observed CP behavior was the interfacial polarization mechanism. The observed increase in the ε′ value, correlated with the enlargement of the average grain size, can be attributed to the effect of the internal barrier layer capacitor. However, when the sintering time ≥4 h, the grain size did not significantly affect the ε′ value, possibly due to reaching the maximum capacity of electron production for the interfacial polarization process (i.e., the maximum intensity of polarizability). This study provides valuable insights into optimizing the sintering conditions for TNTO ceramics and related compounds, laying the groundwork for the development of a new CP oxide suitable for practical applications.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call