Abstract

The Si3N4-BN composites have been prepared via die pressing and the precursor infiltration and pyrolysis route using borazine as the precursor. The Si3N4-BN composites are composed of h-BN, α-Si3N4, and β-Si3N4 produced at a pyrolysis temperature from 1200 to 1750 °C with only 0.17-3.9 wt.% phase transition of Si3N4. The effect of pyrolysis temperature on properties of the composites has been investigated. The density and mechanical properties of the composites, at both room temperature and 1000 °C, increase along with the elevating of the pyrolysis temperature. The density of the composites achieves 2.33 g/cm3 at 1750 °C with the porosity of 14.1%. The flexural strength, elastic modulus, and fracture toughness at room temperature of the Si3N4-BN composites pyrolyzed at 1750 °C are 219.1 MPa, 75.5 GPa, and 2.62 MPa m1/2, respectively. A desirable flexural strength of 184.9 MPa with a residual ratio of 84.4% has been obtained when the composites are exposed at 1000 °C in the air. Micrographs of SEM and TEM illustrate the bonding structure of the pyrolysis BN and Si3N4 grains.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.