Abstract

The effect of pre-weld heat treatment on the microstructure and low-temperature impact toughness of the coarse-grained heat-affected zone (CGHAZ) after simulated welding was systematically investigated through the utilization of scanning electron microscopy (SEM) and electron back-scattering diffraction (EBSD). The Charpy impact test validated the presence of an optimal pre-weld heat treatment condition, resulting in the highest impact toughness observed in the CGHAZ. Three temperatures for pre-weld heat treatment (690, 720 and 750 °C) were used to obtain three different matrices (Steel 1, Steel 2, Steel 3) for simulated welding. The optimal pre-weld heat treatment is 720 °C for 15 min followed by water quench. Microstructure characterization showed that there is an evident microstructure comprising bainite (B) in Steel 1 and Steel 2 after pre-weld heat treatment, while the addition of martensite (M) with the pre-weld heat treatment temperature exceeds Ac1 by almost 60 °C (Steel 3). These differences in microstructures obtained from pre-weld heat treatment influence the refinement of high-temperature austenite during subsequent simulated welding reheating processes, resulting in distinct microstructural characteristics in the CGHAZ. After the optimal pre-weld heat treatment, Steel 2 subjected to single-pass welding thermal simulation demonstrates a refined microstructure characterized by a high density of high-angle grain boundaries (HAGBs) within the CGHAZ, particularly evident in block boundaries. These boundaries effectively prevent the propagation of brittle cracks, thereby enhancing the impact toughness.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call