Na-doped ZnO thin films were deposited on the glass substrates using sol-gel method. The effect of Na concentrations on the structural and optical properties of ZnO films was studied. As Na concentration increases from 0.0 at% to 16.0 at%, preferential c-axis orientation becomes more and more obvious, and the intensity of the diffraction peaks from (103) increases. The optical band gap Eg value increases from 3.261 to 3.286 eV first and then decreases as Na concentration increases from 0.0 to 2.0 at% and then beyond 2.0 at%. The intensity of all the emissions increases with increasing Na concentration and the origins of the violet emission (wavelength in the 400–407 nm) and the blue emission (wavelength at 473 nm) were discussed in detail.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.