In Present work, the properties of Al2O3 powder was studied through incorporation of MgO Nano powder along with ZnO Nano powder and followed by sintering at various temperatures. Previously ZnO and MgO were introduced with Al2O3 separately to improve physical and mechanical properties like densification, micro hardness, fracture toughness etc. In current project, 0.25wt% and 0.50wt% MgO was added with β- Al2O3 matrix along with constant 0.1wt% ZnO and sintered those samples at 14500°C, 15000°C, 15500°C respectively. Properties like densification, micro hardness, and wear rate of all these sintered products were measured and discussed where the best composition found was 0.1% ZnO-0.25%MgO-99.65% Al2O3 sintered at 15000°C. Change in properties was observed due to faster densification rate and pinning effect provided by the doping particles.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.