Abstract In this study, yarn finenesses that are used in the fabric preform, fabric preform density, and preform laying angle were taken as the three important variables, and then the range of the process parameter was also selected based on the pilot run. These selected process parameters and their three different ranges were selected to conduct the experiments. In pure jute composites, the measured properties of tensile strength, flexural strength, and compression strength were very high in the plain-woven composites. This is ascertained through verification of experiments by producing a new sample. Through signal-to-noise ratio analysis, the research found that an optimum flexural value of 85.6822 MPa is obtained by maintaining the process parameter pattern as A1B1C1.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.