Abstract
Recrystallization behaviors have been investigated with respect to two different kinds of the initial structures, original austenite and martensite, in an Fe-32%Ni alloy. The recrystallized austenite grain size from the martensite is much smaller than that from the original austenite, and decreases linearly with increasing the initial hardness, independent of the initial structure. The recrystallization sequences are different between the two structures: only one step due to recrystallization appears in hardness-temperature curve of the original austenite, whereas two steps corresponding to reverse transformation of α’ to r’ and recrystallization are shown in that of the martensite.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.