Abstract

AbstractThe Sn‐Zn alloys have been considered as lead‐free solders. In this paper, the effect of 0.0, 0.5, 1.0, 1.5 and 2.0 wt.% Indium as ternary additions on melting temperature, structure, microhardness and micro‐creep of the Sn‐9Zn lead‐free solders were investigated. It is shown that the alloying additions of Indium to the Sn‐Zn binary system result in a suppression of the melting point to 187.9 °C. From x‐ray diffraction analysis, a new intermetallic compound phase, designated β‐In3Sn is detected. The formation of an intermetallic compound phase causes a pronounced increase in the electrical resistivity and mechanical strength. Also, an interesting connection between dynamic Young's modulus and the axial ratio (c/a) of the unit cell of the β‐Sn was found in which Young's modulus increases with increasing the axial ratio (c/a). The ternary Sn‐9Zn‐xIn exhibits creep resistance superior to Sn‐9Zn binary alloy. The better creep resistance of the ternary alloy is attributed to solid solution effect and precipitation of In3Sn in the Sn matrix. The addition of small amounts of In is found to refine the effective grain size and consequently, improves hardness. The 89%Sn‐9%Zn‐2%In alloy is a lead‐free solder designed for possible drop‐in replacement of Pb‐Sn solders. (© 2010 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim)

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.