Abstract

The effect of hot rolling on the structure and mechanical properties of three Mg–Y–Zn–Mn alloys was studied depending on the process temperature and the reduction ratio. The original plates of cast WZM111, WZM211, and WZM321 alloys after heat treatment were subjected to rolling from an initial thickness of 7 mm to a final thickness of 0.2 mm at two temperatures, namely 400 and 450 °C. Optical and scanning electron microscopy, the microhardness measurement, and tensile testing were used to characterize the material. The rolling regimes that provide a good balance between the strength and ductility of the alloys were established.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.