Abstract The 9CrODS steel specimens were prepared by different processing with hot-rolling and different cooling rate. The hardness and high-temperature tensile properties were measured. Microstructure was analyzed by means of EBSD inverse pole figure and kernel average miss-orientation angles. The hot-rolled and then air-cooled specimen has the highest tensile strength. The furnace-cooled specimen also has better tensile strength at 700 °C than air-cooled specimen at normalized condition. The high-temperature strength of 9CrODS steel is significantly improved with increasing grain size that can be induced by hot-rolling or furnace-slow cooling, where the localized grain boundary deformation can be suppressed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.