Abstract

Abstract—This work studies the effect of heat treatment on the magnetoimpedance (MI) effect of soft magnetic Co68.5Fe4Si15B12.5 amorphous ribbons prepared by melt quenching on a rotating wheel. It was found that after heat treatments at temperatures of 100°C and higher there occur irreversible changes of MI over a wide range of excitation ac frequencies. A change in the magnetoimpedance response to the action of elastic tensile stresses is shown to be related to the change in the sign of saturation magnetostriction coefficient (λS), which results from the heat treatment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.