Abstract

Carbon fiber-reinforced composites were manufactured by hot pressing stacked carbon fiber prepregs using graphene oxide (GO)-modified epoxy resin as the matrix. Tetrahydrofuran was used as the solvent to disperse GO in the epoxy resin. Results showed that a homogeneous GO-modified epoxy system could be obtained, which was stable for approximately 3 h, long enough to produce the prepreg. The incorporation of 0.10 wt% GO into the epoxy resin achieved the largest interlaminar shear strength (ILSS) of 96.14 MPa for laminates, 8.05% higher than that without GO. Also, the glass transition temperature of the composite was increased by approximately 5 °C. The improvement of ILSS could be attributed to the toughening of the epoxy resin and an improvement in the interfacial adhesion between carbon fibers and epoxy matrix.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.