Abstract

AZ91 Mg alloys were processed by equal channel angular extrusion (ECAE) up to 4 passes through route-R. The increase in number of ECAE passes to yield fine-grain structure in the bulk Mg alloy with a more dislocation density, this enhances mechanical properties and corrosion resistance. Indeed, microstructural observations revealed an equiaxed and significant grain refinement after ECAE-4P, with a mean grain size (d) of ∼ 4.36μm. Further, the tensile strength, micro-hardness and corrosion resistance were also increased, however the elongation was reduced with the increasing of ECAE passes. The electrochemical polarization test in 3.5wt % NaCl solution revealed a noticeable enhancement in the corrosion resistance of ECAE processed AZ91 Mg alloy compared with the as-received Mg alloy. This is mainly due to grain refinement and distribution of secondary phase particles in Mg alloy matrix during ECAE-4P.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.