Abstract

Four Er-doped LiYF4 crystals with different Er-concentrations were grown by Czochralski method. The laser crystals were characterized by measurements of ICP-AES, XRD, absorption spectra, up-conversion fluorescence spectra, near-infrared (NIR) and mid-infrared (Mid-IR) fluorescence spectra, as well as luminescence decays. It was found that the heavily 15at% Er-doped YLF crystal is more proper in up-conversion or ∼3μm laser applications; while the 5at% Er-doped YLF is a better candidate for ∼1.5μm lasers within these four crystals.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.