Abstract

The Dy x Pr 2- x Fe 17 ( x =0.0, 0.1, 0.2, 0.3, 0.4) powder was prepared by arc-smelting and high energy ball milling. The phase structure, morphology, magnetic properties and electromagnetic parameters of the powder were investigated by X-ray diffraction (XRD), scanning electron microscopy (SEM), vibrating sample magnetometer (VSM) and vector network analyzer (VNA), respectively. The results reveal that the saturation magnetization of the Dy x Pr 2- x Fe 17 alloys decreases with the increase of Dy content. The minimum absorption peak frequency shifts towards higher frequency region upon the Dy substitution. And the minimum reflection loss of the Dy x Pr 2- x Fe 17 alloys increases firstly and then decreases upon the Dy content. The Dy 0.3 Pr 1.7 Fe 17 powder exhibits the best microwave absorbing properties. The minimum reflection loss of Dy 0.3 Pr 1.7 Fe 17 powder is about −42.38 dB at 5.04 GHz, and the frequency bandwidth of R L <−10 dB reaches about 1.20 GHz with the best matching thickness of 2.5 mm.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call