Abstract

Characterizations of oxide films formed on 316 stainless steel in high temperature, hydrogenated water were conducted. The results show the oxide film consists of an outer layer with oxide particles of Fe–Ni spinel and hematite, and an inner continuous layer of Fe–Cr–Ni spinel. Increasing dissolved hydrogen (DH) concentrations causes decrease of Cr- and increase of Fe-concentrations in the inner layer. A continuous decrease of Cr- and increase of Fe-concentrations was observed from the surface of the inner layer to the oxide/substrate interface. The DH effect is attributed to the enhanced diffusion of Fe ions in the oxide film by hydrogen.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.