An atmospheric-pressure spatial atomic layer deposition system operated in atmospheric-pressure spatial chemical vapor deposition conditions is employed to deposit alumina (AlO x ) thin films using trimethylaluminum and different oxidants, including water (H2O), hydrogen peroxide (H2O2), and ozone (O3). The impact of the oxygen precursor on the structural properties of the films and their moisture-barrier performance is investigated. The O3-AlO x films, followed by H2O2-AlO x , exhibit higher refractive indexes, lower concentrations of OH− groups, and lower water-vapor-transmission rates compared to the films deposited using water (H2O-AlO x ). The AlO x films are then rapidly deposited as thin-film-encapsulation layers on perovskite solar cells at 130 °C without damaging the temperature-sensitive perovskite and organic materials. The stability of the p–i–n formamidinium methylammonium lead iodide solar cells under standard ISOS-D-3 testing conditions (65 °C and 85% relative humidity) is significantly enhanced by the encapsulation layers. Specifically, the O3-AlO x and H2O2-AlO x layers result in a six-fold increase in the time required for the cells to degrade to 80% of their original efficiency compared to un-encapsulated cells.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.