Abstract
To investigate whether high-level irradiance and short light exposure times with light-emitting diode (LED) curing units could provide bond strength comparable to halogen lights for ceramic laminate veneers (CLVs). A total of 160 extracted human maxillary central incisors were prepared to receive CLVs (lithium disilicate) in shades A1 and A3.5. CLVs were luted with light-curing (LC) and dual-curing (DC) resin cements using four protocols: 3 seconds in extra power mode, 8 seconds in high power mode, or 10 seconds in standard mode with an LED unit, or 40 seconds with a conventional halogen light from all aspects (n = 10). Following thermal cycles, shear bond strength test was performed with a universal testing machine. Data were analyzed using one-way analysis of variance and post hoc Tukey test. Failure modes were classified under a stereomicroscope, and data were analyzed using Pearson chi-square test (P = .050). According to the intragroup comparison of different irradiation protocols, the mean shear bond strength of the A1-LC-10 group was found to be significantly higher than that of the A1-LChalogen group (P = .026). Shear bond strength values of the A1-LC-10 group and A3.5-LC-10 group were significantly higher than that of the A3.5-DC-10 group (P = .003). The A3.5-DC-3, A3.5-LC-3, and A1-DC-8 groups revealed the significantly most adhesive failures, and the A1-LC-8 group revealed the most mixed failures (P < .001). Both light and dark ceramic shades with LC cement combination responded the best to the standard mode of 10-second exposure time with LED application. However, with conventional halogen light application, the highest bond strength values were obtained with DC cement and light ceramic shade combination.
Paper version not known (Free)
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have