Abstract

CVD diamond films were prepared on the cemented carbide substrate by hot filament chemical vapor deposition method. The diamond coatings were observed with SEM and Raman spectroscopy. The results show that the increase of vaccum pressure greatly promotes the continuous increase of grain size, and the impurity content of diamond is decreasing with the increase of vaccum pressure. With the increase of the CH4 concentration, the grain size of diamond decreases continuously and the composition of non-diamond carbon increases, but when the CH4 is more than 3% the grain size does not change obviously. The substrate temperature has a certain influence on the structure and grain size of NCD. The multilayer NCD/MCD coated cutting tool was prepared by controlling the deposition parameters.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.