Abstract

ABSTRACTThe research work was carried out on the end milling of Al 6082-T6 alloy with cryogenic CO2, LN2 and wet conditions. The highest axial force (Fz), normal force (Fy) and feed force (Fx) values were recorded on cryogenic LN2 machining. Use of cryogenic LN2 helped to reduce the cutting temperatures up to 38.29% and 32.8% when compared with wet and cryogenic CO2 conditions, respectively. The conventional fluid coolant offered a better surface roughness value (Ra) over cryogenic coolants at a feed rate of 0.015 and 0.02 mm/tooth and cutting speed of 100 m/min. The workpiece surface quality degraded in cryogenic machining conditions during the slot end milling operation of aluminum alloy under the given machining parameters.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.