The deformation and mechanical properties of Zr-based bulk metallic glasses (BMGs) under a nanoindenter and the effect of cooling rate, the effect of cooling rate, tungsten fiber addition and annealing on them have been studied by means of a nanoindentation instrument and a scanning electron microscope (SEM). The results indicate that the deformation of Zr-based BMGs under a nanoindenter is characterized by multiple shear bands and viscous flow which confirms the existence of a amount of plastic deformation. For pure quenched Zr-based BMGs, the larger the size of samples or the nearer the location away from the surface of a same sample, the smaller the values of microhardness (Hv) and elastic modulus (E); Annealing and tungsten fiber addition enhance the values of Hv and E; meanwhile, they also significantly change morphology around a nanoindenter and the amount of plastic deformation. The mechanism of plastic deformation is preliminarily analyzed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.