Abstract

The amount of copper flash smelting slag has increased during the recent years along with an increasing slag-to-metal ratio. During slag tapping, some copper sulfide is mechanically entrained. As a result, it is necessary to recover copper matte from the slag by suitable methods. At present, the most common way is slow, controlled cooling in a transfer ladle. However, research on the detailed effects of slow cooling and the function of slag modification is rare. This paper described experiments that were performed at different cooling rates (0.5, 1.5, 3, and 7 °C/min), with and without additive. A detailed characterization of the copper-rich phase and its particle size was subsequently made using SEM-EDS micrographs and image analysis software. With a decrease in cooling rate, the particle size of the copper-rich matte phase became larger. The addition of gypsum and carbon as a slag modifier affected the size of the copper-rich phase slightly, and its chemical composition was modified compared with the experiments without additive.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.