Abstract

The aim of this study is to evaluate the properties and microstructure of pure titanium after its chemical heat treatment (CHT) by boriding and nitriding. Nitriding and boriding were both done in powder backfill for ten hours. The temperature of the nitriding was 550 °C. The temperature of the boriding was 1000 °C. Both processes led to the creation of a thin surface layer of nitrides and borides which affected wear resistance and also they affected corrosion resistance of the surface of the analyzed samples.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.