Abstract

The purpose of this in vitro study was to evaluate the surface and resin-dentine interface characteristics of permanent tooth dentine cut with diamond or carbide burs and treated with phosphoric acid (PA) or an acidic conditioner. Labial surfaces of permanent incisors were prepared into dentine with high-speed carbide or diamond burs and divided into two halves. Phosphoric acid 36% was applied on one half and non-rinse conditioner (NRC) was applied on the other half. Ten randomly selected scanning electron microscopy (SEM) fields from each specimen (n = 15) were evaluated. Occlusal surfaces of third molars were divided in two halves for evaluation of the resin-dentine interface. The halves were randomly assigned to one of each conditioner and restored with Prime & Bond NT/Spectrum. Ten specimens were analysed by SEM to evaluate hybrid layer formation and interfacial seal. We observed that surfaces prepared with carbide bur presented less residual smear plugs (P < 0.05) than surfaces prepared with diamond burs. Surfaces conditioned with NRC, which is a smear layer modifier, presented more residual smear plugs than surfaces conditioned with PA (P < 0.05). Treatment with PA resulted in more sealed interfaces than specimens treated with NRC. Within the limitations of this study the results showed that carbide burs leave a surface that is more conducive to bonding than diamond burs.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.