In this experimental study, chromium oxide powder was sprayed on a low-carbon steel substrate using the atmospheric plasma spray process. The current and standoff distances (SODs) were varied to study their effect on the fracture toughness of the coatings. Theoretically, as the arc current increases, the melting of the ceramic oxide should increase and this in turn should lead to the formation of a dense coating. However, it was observed that if the arc power is too high and because the particle size of the powder is small (approximately 30 μm), the particles tend to fly away from the plasma core. Similarly, an appropriate SOD should provide the particles with more melting time, thus resulting in a dense coating. On the other hand, a larger SOD leads to the solidification of the molten particles before the droplets can reach the substrate. All these effects may lead to substantial variation in the fracture toughness of the coating. The present paper attempts to correlate the plasma spraying parameters and microstructure of the coating with the fracture toughness and other primary coating properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.