Abstract

This study investigated the effect of adherend temperature on shear bond strengths of auto-polymerizing resin to denture base resin and 4-META/MMA-TBBO resin to silver-palladium-copper-gold (Ag-Pd-Cu-Au) alloy. Bonding procedure was carried out when adherend temperature was 10, 23, 37, or 55°C, and shear bond strengths (SBSs) were measured before and after thermocycling. Before thermocycling, there were no significant differences in bond strength among the four adherend temperatures for each adhesive resin: 31.59±6.11-32.89±2.12 MPa for auto-polymerizing resin; 35.43±2.2-38.38±0.61 MPa for 4-META/MMA-TBBO resin. After thermocycling, optimal adherend temperature to achieve the highest bond strength was 37°C for auto-polymerizing resin to denture base resin (30.02±2.29 MPa) and 10ºC for 4-META/MMA-TBBO resin to Ag-Pd-Cu-Au alloy (37.14±2.17 MPa).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.