Porous polysulfone (PSf) hollow fiber membranes were fabricated via a phase-inversion method by using low molecular weight additives in the spinning dopes. Polyethylene glycol (PEG200), ethanol, glycerol and acetic acid were used as the additives. An aqueous 95 wt.% 1-methyl-2-pyrrolidone (NMP) solution was used as neutral bore fluid to fabricate inner skinless hollow fibers membranes. The precipitation rate of the polymer dopes with the different additives was studied using cloud point measurement. Effect of the additives on the resulting membrane structure, surface porosity, pore size, critical water entry pressure (CEP w) and CO 2 absorption performance were investigated. Cloud point diagrams indicated that the precipitation rate of the polymer dopes increased following the trend of glycerol > acetic acid > PEG200 > ethanol. Results of gas permeation tests showed that glycerol and PEG200 as additives provided the membranes with the largest and smallest pore size, respectively. Moreover, all the additives resulted in an increase in the surface porosity. The cross-section and inner surface of the membranes were examined via a field emission scanning electronic microscopy (FESEM). Glycerol in the spinning dope provided the membrane structure with a thin finger-like and a thick sponge-like layer, which resulted in a higher CEP w and CO 2 absorption rate than the other PSf hollow fiber membranes.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.