Abstract
Muon spin spectroscopic measurements were made on atactic low-molecular-weight (LMW) (1.3 kg mol−1) and high-molecular-weight (HMW) (202 kg mol−1) polystyrene. Muoniated cyclohexadienyl radicals, which are formed by muonium addition to the phenyl side groups, are used as local probes of bulk dynamics. Muon spin relaxation is caused by the secondary γ-relaxation process, which involves motion of the phenyl rings, and is sensitive to the glass transition. The activation energy of the γ-relaxation process in the rubbery state is 0.60(2) eV in the HMW sample and 0.37(3) eV in the LMW sample.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Similar Papers
More From: Journal of Physics: Condensed Matter
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.