Abstract

SummaryIn all polymer solar cells (all-PSCs), the domain size is critical for device performance. In highly crystalline polymer blends, however, precisely adjusting the domain size remains a significant challenge because of the simultaneous crystallization of both components. Herein, a strategy that promotes acceptor and donor to crystallize separately was proposed. Take PBDB-T/N2200 blends for instance; the solution state and confined crystallization were combined, which induced the crystallization of N2200, and PBDB-T occurred during the film-forming process and at thermal annealing stage. This separated crystallization process lowers the driving force of phase separation without affecting the degree of crystallinity of the blends. Thus, an interpenetrating network with high crystallinity and proper domain size was obtained, which boosted the power conversion efficiency to 7.59%. Importantly, the relation between pre-aggregation and domain size was established, which may be a guide to precisely adjust the active layer’s domain size in all-PSCs.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.