Abstract
Clay samples containing 8.15% iron oxides and 27.49% alumina were leached in oxalic acid. Leaching experiments were performed in aqueous solutions of oxalic acid of 0.2–2 mol/L at 40–80°C for up to 90 min. The mixed kinetic mechanism, i.e., t/τ=[(1–2X/3)−(1−X)2/3]+b[1−(1−X)1/3], seemed to be the most appropriate one to fit the kinetic data of leaching iron oxides contained in clay in the aqueous oxalic acid solutions. The Arrhenius activation energy for leaching in the 1.8 mol/L oxalic acid was found to be 41.035 kJ/mol.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Journal of Minerals, Metallurgy, and Materials
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.