Abstract
The evolution of microtwins during high temperature creep deformation in a γ′ strengthened Ni-based superalloy has been investigated through a combination of creep testing, transmission electron microscopy (TEM), theoretical modeling, and computer simulation. Experimentally, microtwin nucleation sources were identified and their evolution was tracked by characterizing the deformation substructure at different stages of creep deformation. Deformation is highly localized around stress concentrators such as carbides, borides and serrated grain boundaries, which act as sources of a/2〈110〉 matrix-type dislocations. Due to fine channels between the γ′ particles, coupled with a low γ matrix stacking fault energy, the a/2〈110〉 matrix dislocations dissociate into a/6〈112〉 Shockley partials, which were commonly observed to be decorrelated from one another, creating extended intrinsic stacking faults in the γ matrix. Microtwins are common and form via Shockley partial dislocations, cooperatively shearing both the γ and γ′ phases on adjacent {111} glide planes. The TEM observations lead directly to an analysis of dislocation–precipitate interactions. The important processes of dislocation dissociation and decorrelation were modeled in detail through phase field simulations and theoretical analyses based on Orowan looping, providing a comprehensive insight into the microstructural features and applied stress conditions that favor the microtwinning deformation mode in γ′ strengthened Ni-based superalloys.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.