Abstract
AbstractA linear polyurethane of high molecular weight was prepared in solution by the polyaddition of equimolar amounts of ethylene glycol and methylene bis(4‐phenyl isocyanate). The polymer was fractionated by using a direct sequential extraction procedure, with a solvent–nonsolvent system consisting of N,N′‐dimethylformamide (DMF) and acetone (A). The resulting fractions were characterized by viscosity and lightscattering measurements. The relationship between the intrinsic viscosity and molecular weight was found in DMF at 25°C. to be [η] = 3.64 × 10−4M0.71. The unperturbed polymer chain dimensions were determined from intrinsic viscosity measurements carried out under experimentally determined theta conditions.