Abstract

Results of studies of dielectric properties and conductivity in 290–700 K range of temperature and frequencies from 25 to 106 Hz in ferroelectric perovskite solid solutions Li0.07Na0.93Ta0.1Nb0.9 O3 and Li0.07Na0.93Ta0.111Nb0.889 O3 are reported. A first-order ferroelectric phase transition proceeds in both studied compositions within the observed range of temperature. The co-precipitated Ta2yNb2(1-y)O5 pentoxides being used for synthesis of Li0.07Na0.93Ta0.111Nb0.889O3 the Curie point shifts by ∼75 K to a lower temperature while compared with Li0.07Na0.93Ta0.1Nb0.9O3 synthesised from mechanical mixture of the Ta2O5 and Nb2O5 oxides the high-frequency dielectric permittivity and ion conductivity of relatively low value of activation enthalpy increases.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.