Abstract
Electrothermal measurement techniques often require thin dielectric barriers to isolate active electrical test structures from samples of interest. The combined need for electrical passivation but thermal proximity necessitates the use of an electrically thick but thermally thin barrier layer. Here, we demonstrate a hybrid approach toward constructing sub-300 nm SiO2 multilayer barriers based upon low-temperature plasma-enhanced atomic layer deposition and high density plasma chemical vapor deposition. Using pairs of buried metal test structures, we quantify changes in device resistance and cross-talk after covering the dielectric barrier with thin evaporated gold films and thick electroplated copper films. We show that a hybrid approach to passivating electrothermal measurement devices outperforms individual homogenous barriers formed by either deposition technique.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.