ABSTRACT(Pb0.985-xBi2x/3La0.01)(Nb0.95Ti0.0625)2O6 with 2 wt% excess PbO (x = 0, 0.01, 0.04, 0.06, 0.1) piezoelectric ceramics with high Curie temperature were fabricated via a conventional solid-state reaction method. Dielectric and piezoelectric properties of the ceramics were studied. The Curie temperatures of the ceramics decrease with the increase in the Bi3+ amount. The values of dielectric constant remain nearly unchanged from room temperature up to about 400 °C for the ceramics with x = 0, 0.01, 0.04 and 0.06. The ceramic with x = 0.04 possesses high piezoelectric charge constant (87 pC/N), low mechanical quality factor (22.60), low dielectric loss (0.024), and high Curie temperature (494 °C).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.