Abstract

(Pb1-xBax)ZrO3(PBZ) ceramics forx= 0.10 were synthesized by the mixed oxide solid state reaction method. Phase transition was investigated by dielectric measurements in the temperature range from 27 to 350 °C at various frequencies. The permittivity of the solids corresponding to (Pb1-xBax) ZrO3showed the maximum value of 10220 atx= 0.10 at the phase transition temperature. The maximum permittivity gradually increasing concentration up tox= 0.10. The ferroelectric hysteresis loop of the PBZ ceramics forx= 0.10 is displayed at room temperature and 0.2 Hz.