Two differently sized microspheres were sintered at 1300°C and 1400°C from 2 to 8h in stoneware, alumina, yttria and zirconia moulds. Selecting the appropriate material to be used as a mould remains a critical issue given titanium's high reactivity at elevated temperatures. Optimum mechanical properties were obtained when sintering the smallest microspheres in yttria-coated moulds. Stiffness of the samples was lower than 40% of that of the bulk solid material, which comes closer to that of human cortical bone. Open and interconnected porosity was observed in all the specimens.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.