Abstract
Ferric oxalate catalyst supported on phosphoric acid treated kaolin (ATKaol) was prepared and tested on the degradation of 4-nitrophenol (4-NP). The X-ray fluorescence (XRF) and Brunauer–Emmett–Teller (BET) characterization results showed drastic distortions in the raw kaolin (Kaol) crystalline structure and an increase in specific surface area (SSA) from 18.78 to 166.12m2g−1 after acid treatment. The incorporation of Fe was confirmed with Fourier transformed infra-red spectroscopy (FTIR), X-ray diffraction (XRD) and energy dispersive X-ray (EDX) results. The degradation of 4-NP without UV was slower compared to when UV was used. There was no appreciable degradation in the absence of either catalyst or hydrogen peroxide (HP). The acid treated kaolinite catalyst (ATKaolCat) exhibits high catalytic activity without pH adjustment degrading 99% of 4-NP (100ppm) in 4min using 2.0g ATKaolCat and 20% excess HP at 40°C. The reusability study shows 9.4% decrease in efficiency after 5 rounds. The kinetic model developed showed good agreement with the experimental data. The model showed that ATKaolCat has higher selectivity for direct oxidation of 4-NP to mineralized products compared to oxidation via intermediates. These qualities make the catalyst promising in 4-NP degradation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.