Abstract
The dependence of the electrochemical characteristics of a layered cathode material containing LiNi0.5Mn0.3Co0.2O2 on the method for applying a protective layer of nanoparticles of the lithium-conducting material Li1.3Al0.3Ti1.7(PO4)3 with a NASICON structure to its surface has been studied. The surface modification has been found to improve the capacity retention in prolonged charge/discharge cycling (up to 15%) and to allow fast charge/discharge processes. The possibility of using a composite electrolyte consisting of a porous ceramic matrix of aluminum-substituted lithium titanium phosphate Li1.3Al0.3Ti1.7(PO4)3 with a transition layer of liquid electrolyte LP-71 has been shown. The use of a thick composite solid electrolyte results in a slight reduction (∼5–7 mAh g−1) in initial capacity compared to laboratory cells with the widely used Celgard 2400 separator impregnated with liquid electrolyte. Laboratory cells assembled with a composite electrolyte showed higher stability during charge/discharge cycling: after 80 deep charge/discharge cycles, the capacity reduction was ∼12% for cells with a composite electrolyte, while for the reference cell it was ∼23%.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.