Abstract

The problems caused by synthetic plastics have motivated the use of other materials. This research consisted of taking advantage of the banana peel and cellulose from the pseudostem of this plant to obtain a bioplastic. Dry milling was applied to extract the flour and an acid-alkaline treatment for the cellulose. The elaboration of the thermoplastic material did with a mixture design where fixed amounts of shell flour (5 g), 15% NaOH (5 mL), and water (4 mL), varying the concentrations of the plasticizers, which were glycerol and sorbitol. In two of the formulations, was added as filler 0,5 g of cellulose. The bioplastic obtained was characterized according to its thickness, water vapor permeability (WVP), tension force (TF), break time (bt), and biodegradability. The type of plasticizer and the cellulose content did not affect the thickness of the bioplastic, but it did affect the WVP, TF, and bt. WVP decreases when glycerin is used and increases with the addition of cellulose. The best result for WVP was 1,83 x 10-9 g/Pa.s.m in the formulation where only was used glycerol, while the best values for TF, bt, and biodegradability were 2,4 MPa, 17 seconds, and 37,77%, respectively, with 75% sorbitol and 25% glycerol. Expanding the study of the best formulations would allow their use as a replacement for synthetic plastics.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.