Abstract

Lanthania-and yttria-stabilized zirconium oxide ceramics have been examined using High Performance Liquid Chromatography (HPLC), thermal neutron activation (NA) and X-ray Fluorescence (XRF) analyses and thus determine the stabilizer content. Ceramic powders with the composition ZrO2:x mol % La2O3 (x=5, 10, 15, 20 and 33) and ZrO2:x mol % Y2O3 (x=10, 15, 20 and 25) were prepared by the citrate and the co-precipitation techniques, respectively. The lanthanum content was determined by HPLC (x=5.09, 9.78, 14.98, 19.81 and 25.94) and NA (x=5.15, 10.32, 17.25, 21.08 and 27.97) analyses, the yttrium content by HPLC (x=8.5, 13.5, 17.9 and 22.1) and XRF (x=9.9, 15.8, 20.1 and 24.9) analyses. An experimental sequence, based on continuous dilution of ceramic powder solutions, is proposed for preparing samples for HPLC measurements. A swimming pool nuclear reactor is used for NA analysis. The quantitative determinations of yttrium and lanthanum doping levels obtained using those techniques are described.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call