Synchrotron wide angle X-ray scattering (WAXS) was used to measure the glass-transition temperature (Tg) values for various cellulosic materials including a novel cellulose ester. WAXS patterns were obtained of films cast on silicon nitride windows. Two strong scattering peaks were observed that correlated with the intramolecular repeating anhydroglucose unit (d=10.6–14.3Å) and an intermolecular packing spacing (d=4.4–4.5Å). Real-time measurements were made during temperature cycling over a range of 80–160°C at 5°C/min. Significant shifts in position, width and area for the peak assigned to the intermolecular arrangement of the pseudo-linear cellulose mixed-ester chains were correlated with temperature. The calculated Tg mid-points correlated well with Tg values determined by differential scanning calorimetry (DSC). This application of temperature-dependent WAXS measurements shows promise for Tg determination in samples where shallow second-order transitions are observed by DSC and where other techniques are not applicable.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have