Abstract

One of the most used joining methods in the manufacturing industry is welded joints. Welded joints are non-removable types of joints and good mechanical properties are expected from the weld seam after joining. For this reason, it is extremely important that there are no errors, defects or gaps in the weld area. This study is about the detection of defects existing in the welding regions of various machine elements with welded joints by non-destructive testing methods. The advantages and disadvantages of the non-destructive testing methods used in the study are presented.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.