Abstract
Abstract The growth rate of stress corrosion cracking (SCC) was measured for cold-worked, thermally treated Alloy 690 (UNS N06690, CW TT 690) and cold-worked, solution-treated Alloy 690 (CW ST 690) in hydrogenated pressurized water reactor (PWR) primary water under static load condition. Three important patterns were observed. First, intergranular stress corrosion cracking (IGSCC) was observed in CW TT 690 in PWR primary water in the range between 320°C and 360°C; this rate of SCC growth was slower than in CW mill-annealed Alloy 600 (UNS N06600, CW MA 600). No significant IGSCC was observed in CW ST 690 after 5,109 h in hydrogenated PWR primary water at 360°C. This is opposite of the behavior reported in the literature for high-temperature caustic solutions. Second, to assess the role of creep, rates of creep crack growth were measured in air, argon, and hydrogen gas environments using 20% CW TT 690 and 20% CW MA 600 in the range between 360°C and 460°C; intergranular creep cracking (IG creep cracking) wa...
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have