Films of poly(vinyl alcohol), ∼2 nm thick, on silicon, copper and gold substrates were allowed to degrade for up to 800 min during monochromatized Al Kα XPS. Relative initial degradation rates of 1: ∼33: ∼41 were measured for the three substrates, consistent with their yield of photoelectrons and secondary electrons The initial rate of degradation was found to vary linearly with the x-ray intensity.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.