Abstract

Decay kinetics of the luminescence in undoped and La3+- or Cd2+-doped PbWO4 (PWO) crystals has been studied under the excitation with the fourth harmonic light (300nm) of a femtosecond laser at room temperature. The measurements are carried out by making use of a combination of a monochromator and a streak scope. The intrinsic “blue” luminescence at 440nm in undoped PWO exhibits two fast decay components (1.5 and 13ns). In addition, there appears a rise component of about 60ps. The luminescence and decay characteristics of the doped PWO are essentially the same as those of the undoped one, i.e., there is no appearance of the extrinsic “green” luminescence in the later stage by doping of La3+(1350atppm) or Cd2+(1at%) ions. It is found that the blue luminescence is enhanced in intensity by several 10% in these doped crystals. The influence of dopant ions on the decay kinetics and the luminescence intensity will be discussed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.