Abstract

This paper describes and evaluates accelerated aging of a titanium dioxide (TiO2) filled polyamide (PA) based backsheet film for photovoltaic (PV) modules. Damp heat exposure (85%RH, 85 °C) was carried out up to 2000 hrs. The backsheet was characterized using microscopic, spectroscopic, thermoanalytic, chromatographic, and mechanical methods. While Raman microscopy, infrared spectroscopy in attenuated total reflection mode (IR-ATR), scanning calorimetry (DSC), and thermal gravimetric analysis did not reveal aging-induced changes, significant yellowing was detected by ultraviolet visible near infrared (UV/VIS/NIR) spectroscopy. Depending on the stabilizer type (UV-absorbers, hindered amine light stabilizers (HALSs), and antioxidants), rather different consumption rates were ascertained by high-performance liquid chromatography (HPLC) and gas chromatography (GC). Although the ultimate mechanical properties decreased significantly, no full embrittlement was obtained after damp heat exposure of up to 2000 hrs. The observed physical and chemical aging mechanisms were classified as within the induction period without premature failure.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.